Planetary Ball Mill PM 100
Grinding of alumina in water with 1 mm grinding balls (left) after 1 hour (blue) and after 4 hours (green) In another trial, the material was first pulverized for 1 hour with 1 mm grinding balls and then for 3 hours with mm grinding balls. In this case, an average size of 76 nm was achieved.